An almost unrivalled combination of chemical inertness, thermal stability and low friction earns PTFE its place in the most demanding of applications. Yet this super-polymer has one well-known mechanical weakness that catches designers out more often than any other: cold flow. Also known as creep, cold flow is the slow, permanent deformation of a material held under a constant load. In PTFE it occurs even at room temperature and at stresses well below the material’s short-term strength, which is why a seal, seat or bearing that performs perfectly on installation can begin to leak or lose alignment months later.
Creep has long been PTFE’s Achilles’ heel, ruling it out of applications where it might otherwise check every box. Understanding why PTFE creeps, and how filled grades, modified resins and sensible design can counter it, is essential for anyone specifying PTFE components for long-term, load-bearing service.
What Is Cold Flow?
PTFE is usually referred to as a ‘soft polymer’. Indeed, it exhibits an almost waxy feel and as machinists, one of the first things we learn is to machine PTFE using techniques developed for wood.
This softness implies that when a load is first applied to a PTFE part, it deforms immediately. If the load is maintained, the part continues to deform, initially at a relatively high rate that slows over time. In many applications the deformation eventually levels off, but a portion of it is permanent: when the load is removed, the part does not fully return to its original dimensions.
Cold flow should not be confused with thermal expansion. Expansion is reversible and disappears as the part cools; cold flow is a mechanical deformation that remains. A related phenomenon, stress relaxation, is its mirror image. Where a part is held at a fixed compression, as in a bolted gasket, the stress within it gradually falls. In practice, both effects reduce the force a PTFE component can exert against its mating surfaces.
Why PTFE Is So Susceptible
Chain structure: PTFE is a linear polymer with no cross-links between its molecular chains. The fluorine atoms that give it its chemical inertness also produce very weak forces between neighbouring chains, allowing them to slide past one another under sustained stress. In fact, the same properties that give PTFE its incomparably low coefficient of friction also contribute to its creep.
Temperature: Creep accelerates as temperature rises. PTFE is commonly rated for continuous service up to around 250°C when unloaded, but the temperature at which it can carry a significant load without excessive deformation is considerably lower.
Stress and time: The extent of creep depends on three variables: the stress applied, the temperature, and the length of time the load is held. A part that is perfectly acceptable under a light, intermittent load may deform unacceptably under a heavier, continuous one.
Where Cold Flow Causes Problems
Flange gaskets: As a PTFE gasket thins under bolt load, the compressive force on the flange falls, opening a potential leak path. Virgin PTFE gaskets are therefore rarely suitable for high-pressure joints without reinforcement or containment.
Valve seats: In ball and butterfly valves, PTFE seats are held under constant preload against the closure member. Cold flow erodes that preload, and a deformed seat cannot recover its shape; the only remedy is replacement.
Seals: Under pressure, PTFE seals can extrude into the clearance gap between mating hardware, particularly at elevated temperatures, resulting in damage and loss of sealing.
Bearings and slide plates: Structural bearings and slide plates carry high, continuous loads, often for decades. Without confinement, the PTFE sliding layer would gradually spread and thin over the life of the structure.
Material Solutions
Filled PTFE: Adding fillers is the most common way to improve creep resistance. The filler particles restrict chain movement and carry part of the load, significantly reducing deformation. Each filler, however, brings its own trade-offs, summarised below.
Filler | Creep resistance | Key advantages | Limitations |
|---|
Glass fibre | Good | Good chemical resistance; economical and widely used | Abrasive to soft mating surfaces; attacked by strong alkalis and hydrofluoric acid |
Carbon | Very good | High compressive strength; performs well in water and steam | Electrically conductive, so unsuitable where insulation is required |
Graphite | Moderate | Low friction; reduces wear on mating parts | Limited gains on its own; usually combined with carbon or glass |
Bronze | Excellent | Highest creep resistance of the common fillers; good thermal conductivity | Reduced chemical resistance, particularly to acids; conductive |
Modified PTFE: Modified PTFE incorporates a small proportion of comonomer that refines the resin’s structure without sacrificing chemical resistance. The result is noticeably lower deformation under load, alongside improved weldability and flex life. This is a significant advantage where fillers would compromise purity, as in semiconductor and pharmaceutical applications.
Alternative polymers: Where the load is too high for any PTFE grade, another material may be more appropriate. PCTFE offers far better dimensional stability under load and is widely used for cryogenic valve seats, while PEEK and PAI (Torlon®) provide much higher stiffness and creep resistance at elevated temperatures, albeit with a higher coefficient of friction.

Design Solutions
Material selection alone rarely eliminates cold flow; good design is equally important.
Confinement: PTFE that is fully enclosed has nowhere to flow. Recessing a PTFE sheet into a steel backing plate, as in bridge bearings, or seating a gasket within a groove, allows the material to carry far higher loads than it could unconfined.
Controlling stress: Designing for a lower bearing pressure, for instance by increasing the contact area, reduces creep directly. Long-term creep data for the specific grade and operating temperature, rather than short-term strength values, should guide these limits.
Anti-extrusion features: Minimising clearance gaps and fitting back-up rings made from a stiffer polymer, such as PEEK, prevents seals from extruding under pressure.
Maintaining load: Spring-energised seals use a metal spring to sustain sealing force as the PTFE jacket relaxes. For bolted joints, re-torquing after the initial relaxation period, where the application permits, restores lost compression.
Conclusion
Cold flow is an inherent property of PTFE rather than a defect, and it need not rule the material out of load-bearing applications. The key is to account for it at the design stage: choosing the right filled or modified grade, confining the material wherever possible, and keeping stresses within the limits that long-term data supports. Where the balance between creep resistance, friction and chemical compatibility is not clear-cut, we work with customers to select the grade and geometry best suited to the application.
Read More
1. PCTFE (Kel-F® Equivalent) – Cryogenic Toughness, Low Permeation and What That Means For Component Design
2. Metal Inserts in Machined Plastic Parts: Bridging the Divide Between Plastic and Metals
3. PFA vs PTFE for Semiconductor Fluid Handling