Among fluoropolymers, PTFE has always been the star. Its chemical inertness, low friction coefficient, and its versatility of application have made it the default answer whenever a design engineer reaches for a fluoropolymer. There are, however, duties where the very attributes that make PTFE attractive elsewhere are disqualifying. Sustained loads expose PTFE’s susceptibility to creep; gas containment is not something that PTFE seals can easily provide, and there are certain dimensional tolerances that PTFE simply will not hold. Polychlorotrifluoroethylene (PCTFE, universally known by its acronym, and to an older generation of engineers by the trade name Kel-F®) exists to serve precisely those cases.
The difference is a single atom. In a molecule of PCTFE, chlorine replaces one of the four fluorine atoms in PTFE. Chlorine is the larger atom, and its presence spoils the tight symmetrical helix that gives PTFE its slipperiness and its tendency to flow under load. This results in a fluoropolymer that sacrifices most of PTFE’s low friction and some of its chemical inertness but gains rigidity, creep resistance, optical clarity and an almost total barrier to gas and water vapour.
What makes PCTFE different
Cold flow resistance: This is the property most frequently responsible for a PCTFE specification. PTFE creeps slowly under the influence of a compressive load at room temperature, which is why bolted PTFE seats become loose and PTFE gaskets need to be periodically retightened. PCTFE exhibits very good dimensional stability under load over a very wide temperature range, and it is this stability that makes it a viable material for seats and back-up rings in permanently loaded assemblies.
Gas and moisture barrier: PCTFE has one of the lowest water vapour transmission rates of any thermoplastic and its permeability to gases is a fraction of that of PTFE. This one property is often the deciding factor in situations where a component must contain a gas rather than just resist a chemical.
Cryogenic toughness: PCTFE is tough and dimensionally stable to about –250°C. It will not embrittle or crack in liquid nitrogen, liquid oxygen or LNG service and it resists creep over the entire range – behaviour that is truly unusual amongst fluoropolymers and is the basis of most of its cryogenic applications. In contrast, while PTFE can certainly withstand these conditions, it sacrifices dimensional tolerance over a wide temperature range, making it unsuitable.
Non-flammability and oxidiser compatibility: PCTFE is UL94 V-0 rated and has a long history of use in liquid oxygen and high-pressure oxygen service where it is one of the very small group of polymers considered acceptable.
Optical clarity: Thin sections of rapidly quenched PCTFE are clear. This is less important for machined components than for film but is a useful diagnostic. Transparency is a direct visual indicator of low crystallinity and thus how a given billet has been processed.
PCTFE vs PTFE – Practical Comparison
The most common parameters determining between the two materials are shown in the table below. Published values for PCTFE vary considerably with grade, molecular weight and thermal history and should therefore be read as indicative ranges and not design values.
Parameter | PTFE | PCTFE |
|---|
Tensile strength | Approx. 25–35 MPa | Approx. 34–39 MPa |
Deformation under steady load | Cold flow pronounced | Much lower; creep resistant |
Coefficient of friction | Approx. 0.03–0.05 | Approx. 0.3 (not a bearing material) |
Upper continuous service temperature | Approx. 250–260°C | Approx. 120–150°C |
Lower service temperature | Approx. –200°C | Approx. –250°C |
Gas and water vapour permeability | Average for a fluoropolymer | One of the lowest of all thermoplastics |
Optical clarity | Opaque, white | Thin quenched sections clear |
Cost relative | Medium | Substantially higher |
Applications of PCTFE
Cryogenic and LNG service: Valve seats, seat inserts, gaskets and stem seals for cryogenic control valves and LNG loading systems where the combination of low temperature toughness, low leakage and creep resistance has no easy substitute.
Oxygen and gas handling: Seats, poppets and diaphragms used in oxygen regulators and high purity gas handling where low permeation and oxidiser compatibility are both required.
Aerospace and defence: Valve components, insulators and instrument parts subject to wide thermal excursions, low pressure and long service intervals.
Semiconductor and analytical instrumentation: Fittings, seats and carrier components where outgassing and moisture pickup must be effectively nil, and where dimensional stability over long dwell times is more important than chemical resistance alone.
Machining PCTFE – The Challenge
PCTFE machines to closer tolerances than PTFE but it is much less forgiving. Three attributes determine the outcome.
Thermal history and crystallinity: PCTFE is semi-crystalline and the degree of crystallinity is very dependent on the rate at which the billet was cooled from the melt. Rapid cooling gives lower crystallinity, more toughness and transparency. Slow cooling gives higher crystallinity, more stiffness and a definitely more brittle part. Thick sections tend to be more crystalline in the centre than at the surface since a thick billet cannot be quenched uniformly. So two components machined from nominally identical stock may behave differently and it is worth qualifying stock by section size rather than by grade alone.
Residual stress and distortion: The heavy cutting releases locked-in stress and the part moves. Where close tolerances are required, we rough machine, allow the component to stabilise, then take a light finishing pass and, where the application requires it, an intermediate stress relieving cycle before finishing. Usually trying to keep up the tolerance all at once is false economy.
Notch sensitivity: PCTFE is a rigid material, and rigid materials encourage crack propagation from stress concentrations. Sharp internal corners, sudden changes in section, and undersized radii have been blamed for field failures. Liberal radii at the design stage cost nothing and are much more effective than any adjustment made later on the machine.
And there is another constraint upstream of all this. PCTFE has a narrow processing window between the temperature at which it becomes processable and the temperature at which it begins to decompose, this limits both the sizes in which stock is moulded and the availability of large sections. Realistic stock dimensions should be compared to component geometry early, not assumed.
Grading and Supply Challenges
Molecular weight and ZST: The major difference between PCTFE homopolymer grades is molecular weight, which is typically measured as Zero Strength Time per ASTM D1430. The higher the ZST, the larger the molecular weight, which provides better toughness and impact resistance but makes the material more difficult to process. Thus the choice of grade is a compromise, not a simple ranking.
Trade names: Kel-F® was the historic trade name under which PCTFE first became widely known, and the term persists in engineering drawings and specifications long after the commercial position has changed. PCTFE homopolymer is presently available under a number of trade names and in most cases where enquiries specify Kel-F® a generic PCTFE equivalent will satisfy the enquiry.
Cost: PCTFE is significantly more expensive than PTFE. The difference is large enough that PCTFE should only be specified where the creep or permeation argument is valid. A filled PTFE grade will generally do the same job for considerably less, for a component not permanently loaded nor required to contain a gas.
Conclusions
PCTFE is not, nor is it intended to be a general-purpose fluoropolymer. It is slower to machine, more expensive, more sensitive to processing history, more limited in available section than PTFE and provides none of PTFE’s bearing performance. Instead, it provides a very special combination – dimensional stability under sustained load, toughness at cryogenic temperatures and a barrier to gas and moisture that no other machinable thermoplastic can match. When an application genuinely needs that combination, there is not much else to consider. The engineering job is not to decide if PCTFE will work, but to be honest about if the application really needs it.
Read More
1. Metal Inserts in Machined Plastic Parts: Bridging the Divide Between Plastic and Metals
2. PFA vs PTFE for Semiconductor Fluid Handling
3. Short Neutral Sections in Railways Inside the PTFE Insulating Member